For this build’69 Camaro · street/strip · 6–7k RPM’69 Camaro · 6–7k
50 hours of hand work
JD
Jim DraperFrom his shop notes · draft, Jim’s review pending

Lifter valley · the 357
About 50 hours, by hand, after the machine work. A die grinder with carbon steel bits and a cartridge roll kit. Every parting line deburred, the lifter valley ground to bare metal, the drain returns opened up.

Lifter valley · the 357
The sequence
- Deburr the parting lines
Every casting seam, inside and out.
- Grind the lifter valley to bare metal
Die grinder and carbon steel bits, then the cartridge rolls.
- Open the drain returns
So oil gets back to the pan.
- Tap the oil drip holes
For the oil-hole breather plugs. Plug typeConfirming with Jim
- Pin locks and copper freeze plugs
Freeze plug type TBCConfirming with Jim
What Jim names for it
JD
Jim’s pick comingDie grinder + carbon steel burr set
Jim names the brand he runs. Until then we list nothing.
JD
Jim’s pick comingCartridge roll kit
Jim names the brand he runs. Until then we list nothing.
The full how-to is on the way: grit order, where not to grind, how long each area takes.
Affiliate links. We may earn a commission at no cost to you. As an Amazon Associate I earn from qualifying purchases.